Quick answer: Match the method to the material. Glass: pure water with soft brushes or traditional squeegee, and no abrasive scrapers on toughened or coated glass. Powder-coated or anodised aluminium: a pH-neutral detergent, soft brushes and a clean-water rinse, with no solvents or abrasives. Render: a low-pressure soft wash with biocide for algae. Stone, brick and terracotta: the gentlest method that works, proven on a trial panel, such as nebulous spray, poultice or low-pressure steam, and never high-pressure jet washing. Most buildings have several materials, so one building often needs three or four methods.
Material-by-material guide
Glass and curtain walling
- Use: pure water (RO/DI) and soft brushes, or traditional washing and squeegee.
- Avoid: metal scrapers and abrasive pads, especially on toughened (tempered) glass, where fabrication debris can cause scratching if dragged. Avoid harsh chemicals on coated or self-cleaning glass.
- Also clean: frames, transoms and pressure caps, which collect grime that runs back onto the glass.
- Frequency: every 1–3 months (ground floor and entrances) and 3–4× a year (upper levels).
Powder-coated aluminium
- Use: pH-neutral detergent, soft cloth or brush, and a clean-water rinse.
- Avoid: solvents, strong alkalis and acids, abrasives, and high pressure.
- Why it matters: manufacturer guarantees commonly require regular cleaning, typically every 6–12 months and more often near busy roads.
Anodised aluminium
- Use: neutral detergent and soft, non-abrasive pads.
- Avoid: alkaline cleaners, which can etch the anodic film.
Render (cement, silicone, acrylic, through-coloured)
- Use: a low-pressure soft wash with a suitable biocide to kill algae and lichen, then a gentle rinse.
- Avoid: high pressure, which can erode the surface, break the bond and drive water behind the render (especially on insulated render systems).
- Tip: recurring green streaks point to a water problem, such as poor drips or failed sills. Fix the cause too.
Natural stone (e.g. Portland, Bath, sandstone, granite)
- Use: the least aggressive effective method, chosen by trial panel: nebulous water spray, poultices, low-pressure superheated steam, and specialist low-pressure abrasive only on robust stone.
- Avoid: acids on limestone, alkalis on some sandstones, and high pressure.
- Standard: BS 8221-1.
- Listed buildings: consent may be needed.
Brick and terracotta / faience
- Use: gentle steam or low-pressure methods, with a trial first. Glazed terracotta needs particular care to avoid crazing and damage to the glaze.
- Avoid: acid cleaners on unsuitable bricks (risk of staining), and high pressure on mortar joints.
Quick reference
| Material | Method | Never |
|---|---|---|
| Glass | Pure water / traditional | Metal scrapers on toughened glass |
| Powder coat | Neutral detergent | Solvents, abrasives |
| Anodised | Neutral detergent | Alkalis |
| Render | Soft wash + biocide | High pressure |
| Limestone | Nebulous spray / poultice / steam | Acids, high pressure |
| Sandstone | Steam / trial-proven method | High pressure, unsuitable chemicals |
| Brick | Steam / low pressure | High pressure on joints |
| Terracotta | Gentle, trial-proven | Abrasives on glaze |
FAQ
Can one contractor clean all of these?
Yes, if they have the competence and kit for each. Ask how they'd treat each material on your building.
Does cleaning void cladding warranties?
The wrong cleaning can. The right, documented cleaning often helps keep the warranty valid. Check your O&M manual.
What about graffiti?
Removal depends on the material and the paint. Specialist removers and low-pressure steam are common, and anti-graffiti coatings can help prevent it returning.
Get a material-by-material plan
See our façade cleaning and building maintenance, or request a site survey. Related: pure water vs pressure cleaning.
Sources
- BS 8221-1:2019; Historic England cleaning guidance.
- Glass and Glazing Federation guidance on cleaning glass (toughened glass scratching).
- Typical powder-coating and anodising manufacturer maintenance guides.