Quick answer: London façades go grey and black mainly from traffic particulates (soot and black carbon) and, on limestone such as Portland stone, historic black gypsum crusts formed by sulphur pollution. These can usually be reduced or removed with gentle, material-specific methods: nebulous water spray, poultices, low-pressure superheated steam or controlled low-pressure vortex cleaning. The right one is always chosen by trial panel, following BS 8221-1. Some staining, such as iron staining, deep-set crusts and damaged stone, can't be fully removed without harming the stone. Listed buildings may need consent before cleaning.
What's causing the staining?
| Staining | Typical cause | Where you see it |
|---|---|---|
| Grey/black film | Diesel and traffic particulates | Road-facing elevations, lower floors |
| Black crusts | Gypsum crust from historic sulphur dioxide, trapping soot | Sheltered parts of limestone: under cornices, in recesses |
| Streaking | Water channelling dirt down the façade | Below sills, copings and ledges with poor drips |
| Green/black growth | Algae and lichen | North faces, under trees, damp areas |
| Orange/brown | Iron from corroding cramps or fixings | Around joints and fixings, a sign of a possible defect |
Rust-coloured staining is a warning sign, not just a cleaning issue. Investigate it. See ten signs your façade needs an inspection.
Cleaning options
| Method | Good for | Limits |
|---|---|---|
| Nebulous water spray | Softening crusts on limestone | Slow; uses water; needs careful control in winter |
| Poultices | Localised stains, crusts and some salts | Slow; small areas |
| Low-pressure superheated steam | Soot, grime and biological growth on stone and brick | Not for every coating or fragile surface |
| Low-pressure vortex (fine abrasive) | Robust stone and brick with ingrained dirt | Needs specialist control; not for soft or decayed stone |
| Chemical cleaners | Some brick and granite | Risk of residues, salts and damage; specialist only |
| Laser | Delicate historic and sculptural stone | Specialist conservation work; slow and expensive |
What to avoid: high-pressure jet washing and aggressive abrasives on stone. They remove the stone's surface along with the dirt, and the newly roughened surface soils faster.
The limits: what cleaning can't do
- Iron staining inside stone often can't be fully removed.
- Deep crusts that have replaced the stone's original surface can't be removed without exposing weaker stone. Conservation practice is often to reduce rather than remove them.
- Decayed stone may need repair, not cleaning.
- Cleaning reveals defects such as cracks, open joints and failed repairs. Budget for some repair.
Consent and conservation
If the building is listed or in a conservation area, cleaning that could affect its character may need listed building consent. Talk to the local authority conservation officer early, and use a trial panel to agree the method and the target finish.
FAQ
How often should pollution staining be cleaned?
For stone and brick, a deep clean is typically needed every 5–10 years, with spot cleaning of entrances and ground floors in between. See how often to clean commercial façades.
Has ULEZ reduced façade soiling?
Lower vehicle emissions should reduce new soot deposition over time, but busy-road elevations still soil much faster than sheltered ones.
Can the façade be protected after cleaning?
Anti-graffiti and some protective treatments exist, but treatments on stone need careful specification so they don't trap moisture. Take specialist advice.
Get a trial panel
See our façade cleaning and building maintenance, or request a site survey.
Sources
- BS 8221-1:2019.
- Historic England, guidance on cleaning historic masonry.
- Planning (Listed Buildings and Conservation Areas) Act 1990.