Quick answer: Efflorescence is the white, powdery or crusty deposit that appears on brick, stone, concrete and render. It is made of soluble salts that water carries to the surface and leaves behind as it evaporates. The salts are the visible part. The real problem is the moisture. Brushing the deposit off treats the symptom, but it returns until the water source is found and fixed. So: find where the water is coming from, repair it, let the wall dry, then clean off the salts, preferably dry first. Heavy or repeated salt deposits can also cause flaking and spalling, so do not ignore them.

What is happening

Three things must be present for efflorescence to appear:

  1. Soluble salts in the masonry, mortar, render or concrete
  2. Water to dissolve them and move them through the wall
  3. Evaporation at the surface, which leaves the salts behind

If any of the three is removed, it stops. In practice the easiest one to remove is the water. Salts in building materials cannot usually be taken out, but they will stop moving once the wall stays dry.

Where the salts come from

  • The bricks, blocks or stone themselves
  • Mortar and render, particularly cement-based ones
  • Concrete and screeds
  • The ground, through rising damp
  • De-icing salts, pollution and, near the coast, sea salt
  • Previous repairs, such as inappropriate cement mortar or cleaning chemicals left in the wall

Where the water comes from

SourceTypical sign
Rain driven into the wallEfflorescence concentrated on exposed elevations
Failed joints, cracks and sealantDeposits next to the defect. See façade sealant failure
Leaking copings, parapets and flashingsStaining below the top of the wall. See parapet, coping and flashing defects
Blocked or leaking gutters and downpipesDeposits below the failed section. See gutter clearance
Rising dampSalt band at low level
Condensation or internal moistureDeposits in sheltered or poorly ventilated areas
New construction water"New building bloom" in the first months, which often fades as the wall dries

Where the source is not obvious, a proper investigation is needed. See façade leak investigation.

Why it matters

Efflorescence is often only cosmetic. But salts that crystallise inside the material, called sub-efflorescence, can create pressure that breaks the surface off. The result is flaking brick faces, crumbling mortar and spalling render. Salts can also push paint and coatings off the wall. If you see deposits together with powdering, flaking or damaged surfaces, treat it as urgent.

What it is not

Not every white deposit is efflorescence. Other causes include:

  • Lime bloom or carbonation deposits from cement, which are harder, do not dissolve easily and can need different treatment
  • Mineral deposits from run-off over metal or concrete
  • Paint chalking or old coatings breaking down
  • Mould or algae with a pale appearance. See algae, moss and biological growth

A simple test is whether the deposit dissolves in water: efflorescence usually does, and lime bloom often does not. If in doubt, ask someone to look at it.

How to treat it properly

  1. Find and fix the water source. Repair joints, cracks, copings, flashings, gutters and drainage.
  2. Let the wall dry. This can take weeks or months for a saturated wall.
  3. Dry-brush the deposits off with a stiff brush. Collect the salts. Washing them straight back into the wall just re-dissolves them.
  4. Wash only if needed, with minimal water, and allow it to dry before judging the result.
  5. Repeat dry brushing if salts keep appearing as the wall dries.
  6. Only then consider repairs or coatings. A coating over a wall that is still wet or salty will usually fail. See façade waterproofing coatings.

Avoid acid cleaning unless a specialist recommends it. Acids can damage masonry and leave their own salts behind. Avoid sealing the surface with an impermeable coating before the wall has dried.

When to get help

Call someone with experience of building fabric if:

  • the deposits keep returning after cleaning
  • the wall is flaking, powdering or spalling
  • the cause is unclear
  • the building is old, listed or in a conservation area, where inappropriate treatment can do lasting harm. See listed buildings and conservation areas
  • you see similar deposits in many places, suggesting a wider moisture problem

FAQ

Is efflorescence harmful?

The salts themselves are not usually a safety hazard. The damage comes from the moisture and, in some cases, from salt crystallisation breaking the surface.

Will it go away on its own?

New-building bloom often does as the wall dries. If the moisture source remains, it will come back.

Can I power-wash it off?

Pressure washing may remove it temporarily, but it adds water and can drive salts and moisture deeper. Dry brushing first is usually better.

Can painting over it hide it?

Not for long. Salts and moisture can push the paint off. Deal with the cause first.

Talk to us

If you can see white deposits, send us photographs and the building address. We can inspect the likely sources of water from above, and tell you what we find. Read about our waterproofing and building maintenance services, or request a site survey.

Sources

  • BRE guidance on damp, salts and efflorescence in masonry.
  • Historic England guidance on traditional masonry and damp.
  • Manufacturer guidance for any cleaning, repair or coating products used.
Keep reading

More guides

When Is Rope Access the Right Choice for High-Level Building Work?

Is rope access right for your job? A task-by-task guide to what it does well, where it struggles and when scaffold or a MEWP is better.

Read the guide →

When Should a Building's Anchor Provision Be Reviewed?

Beyond the annual BS 7883 inspection, seven situations mean your roof anchors need reviewing, such as refurbishment, new plant and missing records.

Read the guide →

When Cleaning Is Not Enough: Signs a Façade Needs Repair

A façade clean often uncovers defects the dirt was hiding: cracks, open joints, failed sealant, rust and spalling. What each means and what to do next.